Analysis Note
  • Carbon content: 17.0 - 18.6 %
  • Pressure: ≤ 15 bar
  • stability testing: passes test
  • Performance (anthracene)
  • Theoretical Plates (N/m) (Anthracene): ≥ 80000
  • Capacity factor (Anthracene): 3.6 - 4.6
  • Tailing (USP): 0.90 - 1.55 %
  • Selectivity separation factor (anthracene/progesterone): 1.95 - 2.35